Measurement of radio transparency of polycrystalline CVD-diamond in millimeter-wave range by free-space method
Gnatyuk D. L.1, Zuev A. V.1, Krapukhin D. V.1, Maltsev P. P.1,2, Sovyk D. N.3, Ralchenko V. G.3
1 Institute of Ultra High Frequency Semiconductor Electronics of RAS, Moscow, Russia
2MIREA - Russian Technological University, Moscow, Russia
3Prokhorov General Physics Institute of the Russian Academy of Sciences, Moscow, Russia
Email: dgnatyuk@yandex.ru

PDF
Radio transparency of polycrystalline CVD-diamond disks with diameter up to 75 mm in millimeter-wave range was measured by free-space method. The structure of the disks was characterized by Raman spectroscopy and scanning electron microscopy. Dielectric loss tangent of the samples in the frequency range of 50-67 GHz was found to be in the range of 7.5· 10-3-8· 10-2, increasing with frequency. The transmission loss due to the radiation absorption is about 1%. Keywords: millimeter-waves, polycrystalline diamond, radio transparency.
Publisher:

Ioffe Institute

Institute Officers:

Director: Sergei V. Ivanov

Contact us:

26 Polytekhnicheskaya, Saint Petersburg 194021, Russian Federation
Fax: +7 (812) 297 1017
Phone: +7 (812) 297 2245
E-mail: post@mail.ioffe.ru